Printing ABS and PC: Same Problem, Two Different Mechanisms

Nov 21, 2026

Leave a message

Printing ABS and PC: Same Problem, Two Different Mechanisms

ABS and PC are the two materials people reach for when a printed part has to actually work. They are also the two that punish the same mistake - cooling - in different ways. Here is what each one needs, and what to design around.

 

Why these two

Most printing is done to check a shape. ABS and PC are used when the part has a job: a fixture that gets clamped, a housing that sits near a motor, a duct, a bracket that carries a sensor, a cover that gets dropped.

What separates them from PLA and from photopolymers is not strength alone. It is toughness at temperature - the ability to take a knock without shattering, and to hold a screw thread at 80 °C.

ABS

PC

Strength

Good

High

Heat deflection

~90–100 °C

~120–130 °C

Impact

Good, but brittle when cold

Very high, keeps working near freezing

UV

Poor - yellows and embrittles

Moderate, better than ABS

Printing difficulty

Medium: warps, smells

Hard: hot, warps, hygroscopic

Typical use

Fixtures, housings, covers

Load-bearing brackets, parts near heat

Neither material is UV-stable enough for years outdoors. If the part lives in sunlight, specify a UV-stabilised grade or plan a protective coating - the printing process cannot fix that. And if the part must survive 120 °C continuously, ABS is out and PC is the entry point.

IMG8596MOV20261121114026

Warping is the whole story, and it has two mechanisms

Everything difficult about these materials comes from shrinkage during cooling, but the mechanism differs.

ABS shrinks more, and it shrinks late. Bulk shrinkage is on the order of 0.5–0.8%, and the part stays soft over a wide temperature range, so it keeps contracting well after the layer is laid. Long, flat parts curl at the corners; tall parts split from the bed.

PC shrinks slightly less but at a higher temperature. Its glass transition is around 147 °C, so the part is fighting the bed while it is still hot. PC also needs a hotter nozzle and a hotter chamber, which means more thermal gradient across the part and more stress locked in.

The practical consequences are the same: you must slow the cooling, and you must keep the part warm while it is being built. Not "warm-ish" - actually warm.

Parameter

ABS

PC

Nozzle

230–260 °C

260–300 °C

Bed

100–110 °C

100–110 °C

Chamber

40–60 °C

60–80 °C, enclosed

Bed adhesion

ABS slurry, PEI, glue stick

PEI with high bed temp, or adhesive

Enclosure

Strongly recommended

Required

Drying before use

70–80 °C, 4 h

100–120 °C, 4 h or more

An open-frame printer will produce small ABS parts and will fail on anything large. This is not a tuning problem - it is a physics problem.

IMGE1757

The design answers to warping

You cannot fix warping in the slicer. You design around it:

Keep the footprint small and the height moderate. Warping scales with length, and it is the ratio of footprint to height that decides whether the part survives.

Avoid large flat unsupported areas. A 300 mm flat panel will lift; a panel with ribs or a slight crown will not.

Round the corners. A sharp corner is where the contraction force concentrates and where the lift starts.

Use a continuous perimeter. A part made of thin separate walls cools unevenly; a closed loop with internal ribs holds itself.

Give the first layer something to grip - a brim, or a raft on difficult geometry.

Orient so the longest dimension is not across the layers if the part will be loaded in bending.

IMGE8387

Layer adhesion is the weak direction, and it is not a defect

A printed part is stronger in-plane than across the layers, typically 50–80% of XY strength in Z, and lower at low nozzle temperatures or fast printing.

This is a design constraint, not a quality complaint:

Put the load in-plane. A bracket loaded in shear across layers will delaminate; the same bracket loaded along the layers will carry far more.

Add a fillet at any change of direction, so the stress does not concentrate at a layer boundary.

Raise the nozzle temperature slightly and reduce cooling when strength matters more than surface finish - hotter layers bond better.

Increase the extrusion width on load-bearing walls; wider beads give more bonded area per layer.

PC is more forgiving here than ABS, because it bonds better to itself, but it also prints hotter, which makes the surrounding warping worse.

IMGE8389

Moisture: PC's second punishment

Both materials absorb water. PC does it faster and suffers more.

Wet filament shows up as:

Steam bubbles and popping at the nozzle.

Excessive stringing and a rough surface.

A measurable loss of strength - the water breaks the polymer chains at temperature.

Drying is not optional for PC, and it is cheap insurance for ABS. Dry it, then keep it dry: a sealed box with desiccant during the print, especially for a long build.

IMGE8445

Supports and finishing

Supports. ABS can use HIPS as a soluble support - same printing temperature, dissolves in limonene, leaves a clean interface. PC has fewer good options; breakaway supports in the same material are common, and the marks have to be planned onto non-visible faces.

Smoothing. Acetone vapour polishing works well on ABS and gives a glossy, sealed surface. It does not work on PC - acetone attacks polycarbonate, causing crazing and, under stress, cracking. For PC, use sanding and a compatible coating, or design the surface so it does not need smoothing.

Inserts. Threaded brass inserts installed with heat are the reliable answer in both materials. A self-tapping screw into printed ABS works twice; into PC it works once and then cracks along the layer lines.

Painting. ABS takes paint well after a light scuff. PC needs a primer; adhesion is the limiting factor, not the paint.

IMGE8511

Where these parts belong

Good fits:

Jigs, fixtures, nests and soft jaws that see clamping load.

Functional prototypes that must be assembled and used, not just looked at.

Housings and covers near warm components, where PLA would soften.

Ducts, guards and brackets in industrial equipment.

Replacement parts for machines that are otherwise obsolete.

Bad fits:

Anything evaluated on appearance straight off the machine - layer lines are visible; that is what resin printing is for.

Long-term outdoor parts, unless a UV-stabilised grade or a coating is specified.

Continuous service above 100 °C in ABS, or above 120 °C in PC.

Precision fits across a long distance - the process tolerance and the shrinkage compensation will not hold ±0.05 mm over 500 mm.

Volume production - at a few hundred pieces, moulding or machining becomes the cheaper route.

Design rules worth writing down

Feature

Rule

Reason

Minimum wall

1.2 mm, 2 mm for load-bearing

Thinner walls warp and are weak across layers

Rib thickness

0.6–0.8× wall

Equal thickness creates a hot mass and sink

Corner radius

3 mm minimum, more on large parts

Reduces contraction concentration

Hole diameter

Add 0.2–0.4 mm to the nominal

Material shrinks and holes close slightly

Threads

Heat-set inserts, or coarse self-tapping

Fine threads strip and crack along layers

Mating clearance

0.3–0.5 mm on sliding fits

Printed surfaces are rough and slightly oversize

Long unsupported span

Add a rib every 80–120 mm

Limits sag and warp

Text and logos

Raised, 0.6 mm minimum

Engraved text fills and blurs

What to send with an enquiry

1. The model, and the function - clamped, dropped, heated, sealed.

2. The service temperature, because it decides ABS versus PC.

3. Indoor or outdoor, because UV decides whether the part needs a stabilised grade or a coating.

4. Which faces must be flat or fit, so the orientation can be planned around them.

5. Quantity and whether the design will change - a fixture that will be revised twice is a printing job; one that is frozen at fifty pieces may not be.

6. The fastener type, if inserts are needed, so the pocket can be designed in.

 

About the manufacturer

Shenzhen Strongd Model Technology Co., Ltd. prints functional parts in ABS and PC, alongside resin and nylon (SLS/MJF) processes, for robotics, automotive, medical and consumer electronics customers. The 40,000 m² plant in Shenzhen runs nine industrial printers with builds up to 1,500 × 750 × 550 mm, with dimensional inspection under ISO 9001:2015 and IATF 16949:2016. Prototypes ship in 3–7 days; quotations are returned within 8 working hours.

Website: https://www.strongdcnc.com/

Send Inquiry